HITS-X Series - Applications
High-Speed Impact Testing Machines
High-Speed Tensile Test Measurement Data
Data example for plastics
![](/sites/ssi.shimadzu.com/files/d7/ckeditor/an/test/impact/hits-x/5-1.jpg)
Material : Polycarbonate
Flat plate : 5 mm wide x 2 mm thick
Tensile rate : 20 m/s
Data example for aluminum
![](/sites/ssi.shimadzu.com/files/d7/ckeditor/an/test/impact/hits-x/5-2.jpg)
Round rod : 5 mm radius
Tensile rate : 5 m/s
Puncture Impact Measurement Data
Data example for plastics
![](/sites/ssi.shimadzu.com/files/d7/ckeditor/an/test/impact/hits-x/5-3.jpg)
Material : Polycarbonate (t = 2 mm)
Speed : 10 m/s
Data example for aluminum
![](/sites/ssi.shimadzu.com/files/d7/ckeditor/an/test/impact/hits-x/5-4.jpg)
Material : Aluminum (t = 0.75 mm)
Speed : 20 m/s