0

    Shimadzu Energy Dispersive XRF

    industry_environmental_energyDis.png

    The colored elements can be analyzed by XRF. There are multiple advantages to energy dispersive XRF analyzers such as the Shimadzu EDX-7000. It can analyze solids, liquids, and powders with very little sample preparation or pretreatment. The measurement range is low parts per million (depending on the element) to 100%. Analysis times are 1-10 minutes. It sits right on the tabletop and is capable of rapid semi-quantitative analysis without standards, or very accurate quantitative analysis using standards.

     

    Table 1 is a comparison of XRF data with a certified reference cement.

     

      % MgO %Ai2O3 %SO3 %CaO
    XRF
    1.75
    3.95
    21.9
    69.6
    CRM
    1.93
    3.88
    22.4
    67.9

     

    Figure 1 shows the analysis of metals in waste oil.

     