Return to High Speed Mechanical Testing and Imaging Top Page
Recent Publications - High Speed Mechanical Testing and Imaging: Digital Image Correlation
Featured Scientific Journals & Papers
Effect of temperature on high strain-rate damage evolving in CFRP studied by synchrotron-based MHz X-ray phase contrast imaging New!
Xiyao Sun, David Sory, Kai Liu, Bratislav Lukić, David Simonian, Kwan Lok Wong, Alexander Rack, David Chapman, Nik Petrinic, Daniel Eakins, Effect of temperature on high strain-rate damage evolving in CFRP studied by synchrotron-based MHz X-ray phase contrast imaging, Composites Part B: Engineering, Volume 279, 2024, 111445, ISSN 1359-8368, https://doi.org/10.1016/j.compositesb.2024.111445.
Related Products: High-Speed Video Camera
Read/Download
Visualization of end-gas auto-ignition during PREMIER combustion in a dual-fuel gas engine
Nobuyuki Kawahara, Eiji Tomita, Visualization of end-gas auto-ignition during PREMIER combustion in a dual-fuel gas engine, The Proceedings of the International symposium on diagnostics and modeling of combustion in internal combustion engines, 2022, Volume 2022.10, Session ID C9-3, Pages C9-3-, Released on J-STAGE January 25, 2023, Online ISSN 2424-2918, https://doi.org/10.1299/jmsesdm.2022.10.C9-3, https://www.jstage.jst.go.jp/article/jmsesdm/2022.10/0/2022.10_C9-3/_article/-char/en
Related Products: High-Speed Video Camera
Characterization of local mechanical properties of Al/Cu Magnetic Pulse Welded joints under high strain rates using synchrotron X-ray imaging
Benjamin Zielinski, Tarik Sadat, Bratislav Lukić, Grégory Haugou, Hervé Morvan, Alexander Rack, Eric Markiewicz, Laurent Dubar, Characterization of local mechanical properties of Al/Cu Magnetic Pulse Welded joints under high strain rates using synchrotron X-ray imaging, Materials Letters, Volume 337, 2023, 133943, ISSN 0167-577X, https://doi.org/10.1016/j.matlet.2023.133943. (https://www.sciencedirect.com/science/article/pii/S0167577X23001283)
Related Products: High-Speed Video Camera
Read/Download
Mesoscale shock structure in particulate composites
Ravindran, S., Gandhi, V., Lawlor, B., & Ravichandran, G.. (2022). Mesoscale shock structure in particulate composites.
Related Products: High-Speed Video Camera
Read/Download
A Comparison of High-Rate Tensile Failure Methods for Structural Adhesives
Breedlove, E.L., Powers, R., Kennedy, M., Al Tameemi, M., Priester, J. (2023). A Comparison of High-Rate Tensile Failure Methods for Structural Adhesives. In: Mates, S., Eliasson, V., Allison, P. (eds) Dynamic Behavior of Materials, Volume 1. SEM 2022. Conference Proceedings of the Society for Experimental Mechanics Series. Springer, Cham. https://doi.org/10.1007/978-3-031-17453-7_17
Related Products: High-Speed Video Camera
Read/Download
Quantifying Thermal Output of Energetic Materials: LDRD Final Report
Kearney, Sean, Swain, William, Stacy, Shawn, Halls, Benjamin, wwerik,, Marinis, Ryan, Richardson, Daniel, Marsh, Andrew, and Mazumdar, Yi. Quantifying Thermal Output of Energetic Materials: LDRD Final Report.. United States: N. p., 2022. Web. doi:10.2172/1892464.
Related Products: High-Speed Video Camera
Read/Download
Nano-additive manufacturing of multilevel strengthened aluminum matrix composites
Chenwei Shao, Haoyang Li, Yankun Zhu, Peng Li, Haoyang Yu, Zhefeng Zhang3Herbert Gleiter, André McDonald and James Hogan Accepted Manuscript online 19 October 2022 © 2022 The Author(s). Published by IOP Publishing Ltd on behalf of the IMMT
Related Products: High-Speed Video Camera
Read/Download
The Novel "Fracture" Gun at the DEVCOM Army Research Laboratory for Precise, Highly Instrumented Impact Experiments
Meredith, Christopher. (2022). The Novel "Fracture" Gun at the DEVCOM Army Research Laboratory for Precise, Highly Instrumented Impact Experiments.
Related Products: High-Speed Video Camera
Read/Download
High-Speed Imaging Diagnostics of Hypervelocity Projectile-Water Droplet Interactions
G. D. Lukasik, J. A. Rogers, T. E. Lacy, and W. D. Kulatilaka, "High-Speed Imaging Diagnostics of Hypervelocity Projectile-Water Droplet Interactions," in Optical Sensors and Sensing Congress 2022 (AIS, LACSEA, Sensors, ES), Technical Digest Series (Optica Publishing Group, 2022), paper LTu5B.5.
Related Products: High-Speed Video Camera
Read/Download
An explicit phase field method for dynamic fracture
Huilong Rena , Xiaoying Zhuanga , Cosmin Anitescub , Timon Rabczuk - ICILSM 2022
Related Products: High-Speed Video Camera
Read/Download
Damage accumulation mechanisms during dynamic compressive failure of boron carbide
Brendan M.L. Koch, Haoyang Li, Calvin Lo, Jonathan Ligda, James David Hogan, Damage accumulation mechanisms during dynamic compressive failure of boron carbide, Journal of the European Ceramic Society, 2022, , ISSN 0955-2219, https://doi.org/10.1016/j.jeurceramsoc.2022.05.052. (https://www.sciencedirect.com/science/article/pii/S0955221922004101)
Related Products: High-Speed Video Camera
Read/Download
Spatial evolution of nitric oxide in ns-discharges using a 250 kHz optical parametric oscillator
Boris S. Leonov, Anuj Rekhy, Yue Wu, James R. Creel, and Christopher M. Limbach, "Spatial evolution of nitric oxide in ns-discharges using a 250 kHz optical parametric oscillator," Opt. Continuum 1, 1278-1285 (2022)
Related Products: High-Speed Video Camera
Read/Download
V03-08 MECHANISMS OF LASER LITHOTRIPSY REVEALED WITH ULTRAHIGH-SPEED VIDEO MICROSCOPY OF STONE FRAGMENTATION IN AIR AND WATER
Yuri Pishchalnikov, William Behnke-Parks and Marshall Stoller, V03-08 MECHANISMS OF LASER LITHOTRIPSY REVEALED WITH ULTRAHIGH-SPEED VIDEO MICROSCOPY OF STONE FRAGMENTATION IN AIR AND WATER, https://doi.org/10.1097/JU.0000000000002539.08
Related Products: High-Speed Video Camera
Read/Download
Initiation of a Metal/Fluoropolymer Reactive Material Subjected to Dynamic Shear-Compression Loading
B. Miller, S. G. Thoma, J. Kimberley, Prop., Explos., Pyrotech. 2022, e202100353.
Related Products: High-Speed Video Camera
Read/Download
3D optical diagnostics for explosively driven deformation and fragmentation
Daniel R. Guildenbecher, Elizabeth M.C. Jones, Elise M. Hall, Phillip L. Reu, Timothy J. Miller, Francisco Perez, Andrew D. Thompson, James Patrick Ball, 3D optical diagnostics for explosively driven deformation and fragmentation, International Journal of Impact Engineering, Volume 162, 2022, 104142, ISSN 0734-743X, https://doi.org/10.1016/j.ijimpeng.2021.104142.
Related Products: High-Speed Video Camera
Read/Download
Supersonic jet by blast wave focusing
N. Apazidis, S. Sembian, and M. Liverts , "Supersonic jet by blast wave focusing", Physics of Fluids 33, 126101 (2021) https://doi.org/10.1063/5.0068309
Related Products: High-Speed Video Camera
Read/Download
Hypervelocity impact response of monolithic UHMWPE and HDPE plates
Jacob A. Rogers, Aniket Mote, Paul T. Mead, Khari Harrison, Gavin D. Lukasik, Kalyan Raj Kota, Waruna D. Kulatilaka, Justin W. Wilkerson, Thomas E. Lacy, Hypervelocity impact response of monolithic UHMWPE and HDPE plates, International Journal of Impact Engineering, Volume 161, 2022, 104081, ISSN 0734-743X, https://doi.org/10.1016/j.ijimpeng.2021.104081.
Related Products: High-Speed Video Camera
Read/Download
Density, strain rate and strain effects on mechanical property evolution in polymeric foams
Kapil Bharadwaj Bhagavathula, Christopher S Meredith, Simon Ouellet, Dan L Romanyk, James David Hogan, Density, strain rate and strain effects on mechanical property evolution in polymeric foams, International Journal of Impact Engineering, Volume 161, 2022, 104100, ISSN 0734-743X, https://doi.org/10.1016/j.ijimpeng.2021.104100.
Related Products: High-Speed Video Camera
Read/Download
Diminishing comminution of urinary stones with subsequent laser pulses
Yuri A. Pishchalnikov Applaud Medical, Inc., 953 Indiana St., San Francisco, CA 94107, yuri.pishchalnikov@applaudmedical.com William M. Behnke-Parks Applaud Medical, Inc., San Francisco, CA Marshall L. Stoller Dept. of Urology, Univ. of California San Francisco, San Francisco, CA, "Diminishing comminution of urinary stones with subsequent laser pulses", The Journal of the Acoustical Society of America 150, A329-A329 (2021) https://doi.org/10.1121/10.0008467
Related Products: High-Speed Video Camera
Read/Download
Strain-Rate-Dependent mechanical behavior of a non-Equimolar CoCrFeMnNi high entropy alloy with a segmented coarse grain structure
Haoyang Li, Chenwei Shao, Okan K. Orhan, David Funes Rojas, Mauricio Ponga, James D. Hogan, Strain-Rate-Dependent mechanical behavior of a non-Equimolar CoCrFeMnNi high entropy alloy with a segmented coarse grain structure, Materialia, Volume 21, 2022, 101271, ISSN 2589-1529, https://doi.org/10.1016/j.mtla.2021.101271. (https://www.sciencedirect.com/science/article/pii/S258915292100274X) Abstract: The mechanical response of a Co11.3Cr20.4Fe22.6Mn21.8Ni23.9 (wt%) high entropy alloy with a segmented coarse grain structure is investigated using strain-rate-dependent uniaxial compression experiments. The composition is verified using ab-initio simulations by examining thermal stability through the reduction of Gibbs free energy relative to similar equi-molar alloys. The segmented grain structure, combining high-angle coarse-grains with low-angle sub-grains, provides good hardness (∼3 GPa) and strain-hardening (∼2600 MPa/ε). Yield strength shows strain-rate-dependent behavior with high strain-rate sensitivity. Here, the macroscopic deformation is correlated with the microscopic plastic failure mechanisms, facilitated by advanced in situ visualization and analysis. Results reveal that the formation of deformation bands occur before yield, while the interactions between microscopic plastic deformation mechanisms and the low-angle sub-grain boundaries significantly affect the apparent surface deformation features and mechanical properties.
Related Products: High-Speed Video Camera
Read/Download
Ultra-high speed X-ray imaging of dynamic fracturing in cementitious materials under impact
Ultra-high speed X-ray imaging of dynamic fracturing in cementitious materials under impact Bratislav Lukić, Maria Blasone, Yannick Duplan, Pascal Forquin, Emilio Escauriza, Michael Rutherford, David Chapman, Daniel Eakins, Margie Olbinado, Alexander Rack EPJ Web Conf. 250 01014 (2021) DOI: 10.1051/epjconf/202125001014
Read/Download
A liquid breakdown driven non-invasive microjet injection system
Hwichan Ham, Jack J. Yoh, A liquid breakdown driven non-invasive microjet injection system, Medical Engineering & Physics, 2021,
Read/Download
Investigation of the 2D assumption in the image-based inertial impact test
Van Blitterswyk, J, Fletcher, L, Pierron, F. Investigation of the 2D assumption in the image‐based inertial impact test. Strain. 2021; 57:e12369. https://doi.org/10.1111/str.12369
Read/Download
Graphene Formation through Pulsed Wire Discharge of Graphite Strips in Water: Exfoliation Mechanism
Tanaka, S.; Inao, D.; Hasegawa, K.; Hokamoto, K.; Chen, P.; Gao, X. Graphene Formation through Pulsed Wire Discharge of Graphite Strips in Water: Exfoliation Mechanism. Nanomaterials 2021, 11, 1223. https://doi.org/10.3390/nano11051223
Read/Download
Supersonic needle-jet generation with single cavitation bubbles
Appl. Phys. Lett. 118, 134103 (2021); https://doi.org/10.1063/5.0045705 Submitted: 28 January 2021 . Accepted: 15 March 2021 . Published Online: 01 April 2021
Read/Download
Electronegative microchannel guided streamer propagation for in-liquid spark breakdown applications
Appl. Phys. Lett. 118, 103905 (2021); https://doi.org/10.1063/5.0042591 Submitted: 31 December 2020 . Accepted: 18 February 2021 . Published Online: 11 March 2021
Read/Download
Probing inertial cavitation damage in viscoelastic hydrogels using dynamic bubble pairs
Yang, Jin & Cramer, Harry & Buyukozturk, Selda & Franck, Christian. (2021). Probing inertial cavitation damage in viscoelastic hydrogels using dynamic bubble pairs. 10.13140/RG.2.2.17764.50565.
Read/Download
Two-dimensional dynamic damage accumulation in engineered brittle materials
Brendan M.L. Koch, Calvin Lo, Haoyang Li, Tomoko Sano, Jonathan Ligda, James David Hogan, Two-dimensional dynamic damage accumulation in engineered brittle materials, Engineering Fracture Mechanics, doi:
https://doi.org/10.1016/j.engfracmech.2021.107539
Hypervelocity Impact Response of Polyethylene Plates
Jacob Rogers, Paul T. Mead, Khari Harrison, Kalyan Raj Kota, James D. Leaverton, Gavin Lukasik, Waruna D. Kulatilaka, Justin W. Wilkerson, Thomas E. Lacy, Published Online:4 Jan 2021, https://doi.org/10.2514/6.2021-0887
Read/Download
Real-time damage characterization for GFRCs using high-speed synchrotron X-ray phase contrast imaging
Jinling Gao, Nesredin Kedir, Cody D. Kirk, Julio Hernandez, Junyu Wang, Shane Paulson, Xuedong Zhai, Todd Horn, Garam Kim, Jian Gao, Kamel Fezzaa, Francesco De Carlo, Pavel Shevchenko, Tyler N. Tallman, Ronald Sterkenburg, Giuseppe R. Palmese, Weinong Chen, Real-time damage characterization for GFRCs using high-speed synchrotron X-ray phase contrast imaging, Composites Part B: Engineering, Volume 207,
2021, 108565, ISSN 1359-8368, https://doi.org/10.1016/j.compositesb.2020.108565.
AIAA SciTech Forum and Exposition 2023 Papers
An Acoustic Device for Ultra High-Speed Quantification of Cell Strain During Cell–Microbubble Interaction
Pattinson, O., Keller, S., Evans, N., Pierron, F., & Carugo, D. (0). An Acoustic Device for Ultra High-Speed Quantification of Cell Strain During Cell–Microbubble Interaction. ACS Biomaterials Science & Engineering.
Related Products: High-Speed Video Camera
Read/Download
Time-Resolved Stagnation Pressure Measurement Technique in a Rotating Detonation Rocket Combustor
Kevin Dille, Mark Frederick, Carson D. Slabaugh and Stephen D. Heister. "Time-Resolved Stagnation Pressure Measurement Technique in a Rotating Detonation Rocket Combustor," AIAA 2023-1871. AIAA SCITECH 2023 Forum. January 2023.
Related Products: High-Speed Video Camera
Read/Download
Digital Holography for Investigating Front-Edge Instabilities of Liquid Jets in Supersonic Crossflows
Joshua A. Johnson, Suresh Menon and Yi C. Mazumdar. "Digital Holography for Investigating Front-Edge Instabilities of Liquid Jets in Supersonic Crossflows," AIAA 2023-0804. AIAA SCITECH 2023 Forum. January 2023.
Related Products: High-Speed Video Camera
Read/Download
Time resolved visualization of liquid jet interaction with H2-air Rotating Detonations using MHz-rate Diesel PLIF
Venkat Athmanathan, Matthew Hoeper, Austin M. Webb, Robert B. Wang, Sukesh Roy, H. Douglas Perkins, Christopher A. Fugger and Terrence R. Meyer. "Time resolved visualization of liquid jet interaction with H2-air rotating detonations using MHz rate diesel PLIF," AIAA 2023-0573. AIAA SCITECH 2023 Forum. January 2023.
Related Products: High-Speed Video Camera
Read/Download
Angle Optimized Filtered Rayleigh Scattering for the Imaging of Pressure Waves from Laser Generated Surface Sparks at 250,000 Frames per Second
James R. Creel, Boris S. Leonov and Richard Miles. "Angle Optimized Filtered Rayleigh Scattering for the Imaging of Pressure Waves from Laser Generated Surface Sparks at 250,000 Frames per Second," AIAA 2023-0350. AIAA SCITECH 2023 Forum. January 2023.
Related Products: High-Speed Video Camera
Read/Download
Stabilization Effects in Hydromagnetic Plasma Flows
Thomas C. Underwood. "Stabilization Effects in Hydromagnetic Plasma Flows," AIAA 2023-2055. AIAA SCITECH 2023 Forum. January 2023.
Related Products: High-Speed Video Camera
Read/Download
Simulating Hypervelocity Impacts to High-Density Polyethylene
Jacob Rogers, Paul T. Mead, Justin Wilkerson, Thomas E. Lacy and Neil Williams. "Simulating Hypervelocity Impacts to High-Density Polyethylene," AIAA 2023-2021. AIAA SCITECH 2023 Forum. January 2023.
Related Products: High-Speed Video Camera
Read/Download
Modes of Laser Spark Ignition of a Model Rocket Combustor
Ryan Strelau, Mark Frederick, Will C. Senior, Rohan Gejji and Carson D. Slabaugh. "Modes of Laser Spark Ignition of a Model Rocket Combustor," AIAA 2023-2377. AIAA SCITECH 2023 Forum. January 2023.
Related Products: High-Speed Video Camera
Read/Download
Planar Time-Resolved Laser-Induced Incandescence for Particulate Emissions in Premixed Flames at Elevated Pressures
Andy X. Zheng, Sundar Manikandan, Samuel E. Wonfor, Adam M. Steinberg and Yi C. Mazumdar. "Planar Time-Resolved Laser-Induced Incandescence for Particulate Emissions in Premixed Flames at Elevated Pressures," AIAA 2023-2435. AIAA SCITECH 2023 Forum. January 2023.
Related Products: High-Speed Video Camera
Read/Download
High Temperature Gladstone-Dale Coefficient Measurements in a Free-Piston Shock Tube
Gwendolyn Wang, Kyle Daniel, Kyle P. Lynch, Daniel R. Guildenbecher and Yi C. Mazumdar. "High Temperature Gladstone-Dale Coefficient Measurements in a Free-Piston Shock Tube," AIAA 2023-0225. AIAA SCITECH 2023 Forum. January 2023.
Related Products: High-Speed Video Camera
Read/Download
Additional Journals & Papers
- Compression Strength of Borosilicate and Soda-Lime Silicate Glasses Using a Dumbbell- Shaped Specimen
- Use of Edge-on Impact Tests with Synchrotron-Based MHz Radioscopy to Investigate the Multiple Fragmentation Process in SiC Ceramics
- Mode-I behavior of adhesively bonded composite joints at high loading rates
- Impact failure in two silicates revealed by ultrafast, in situ, synchrotron X-ray microscopy
- The Utility of 3D Digital Image Correlation for Characterizing High-Rate Deformation
- Collapse dynamics of spherical cavities in a solid under shock loading