0

    510

    Loading Unit : Loading Method

    Electromagnetic force

    Indenter : Upper pressure indenter

    Type: Flat indenter (50 µm diameter)
    (500 µm flat indenter as option)
    Material: Diamond

    External Dimensions

    Tester: Approx. W 355 × D 405 × H 530 mm Control unit: Approx. W 315 × D 375 × H 110 mm

    Utilities : Humidity

    80% max. (no condensation)

    Utilities : Vibration

    Horizontal vibration: 0.017 Gal max. (at 10 Hz or more)
    0.01 µm max. (at less than 10 Hz)
    Vertical vibration: 0.010 Gal max. (at 10 Hz or more)
    0.005 µm max. (at less than 10 Hz)

    Utilities : Temperature

    Recommended temperature: 23 ± 1°C Allowable range: 10°C to 35°C

    Utilities : Grounding*1

    The grounding pins of 3-pin connectors must be connected to a resistance of 100 W or less.

    Utilities : Power Consumption

    Approx. 100 W (not including power consumption of PC)

    Available test parameters : Test mode

    Single phase AC 100–115 V ± 10%, AC 230 V ± 10% (Ground resistance 100 Ω max.)

    Available test parameters : Test mode

    Calculation of compressive strength, display of test parameters and results
    Display of test force and displacement data
    Display of test force/displacement curve
    Display of test force/displacement identification value
    Display of strength/particle diameter curve
    Display of displacement/time curve
    Display of strength/parameter curve

    Available test parameters : Test mode

    Particle, fiber or other shapes

    Available test parameters : Test mode

    Compression test, load-unload test, cyclic test

    Specimen stage : Horizontal positioning range

    25 mm for both X and Y directions
    Min. increment: 0.01 mm (0.001 mm with option)

    Specimen Stage : Area

    Approx. W 125 mm × D 125 mm

    Specimen stage : Vertical positioning range

    Approx. 60 mm

    Indenter : Lower pressure plate

    SKS flat plate (Diamond pressure plate available as option)

    Optical Head : Min. increment

    0.01 µm / pulse

    Loading unit : Loading range (mN)

    9.8 – 4903

    Optical monitor : Total magnification

    Approx. × 100, × 500 (× 200, × 400, × 1000 with option)

    Loading unit : Load Accuracy

    Within ± 1% of displayed test force or 0.1 mN (whichever is greater)

    Loading unit : Resolution (µm)

    5 (when testing at 49 mN or less)

    Displacement measurement unit : Method

    Differential transformer

    Displacement measurement unit : Method

    0 – 100

    Displacement measurement unit : Method

    0.001

    Displacement measurement unit : Method

    Within ± 2% of full scale

    Optical Monitor : Objective Lens

    × 10, × 50 (× 20, × 40, × 100 with option)

    Optical Head : Effective measurement range

    Approx. 200 µm (with × 50 objective lens)

    Optical Monitor : Eyepiece

    × 10

    Optical monitor : Illumination method

    Epiluminescent

    Optical monitor : Illumination method

    LED 3 W / 3 V

    Optical monitor : Light path

    Switching between observation and photography possible

    Optical Head : Collimation method

    Direct connection between encorder and control handle: synchronized movement of two indexes

    Optical Head : Detector

    Optical encoder

    Weight

    Tester: Approx. 60 kg Control unit: Approx. 5 kg

    *1 This product is a precision measuring device. Special consideration is required for the product's installation conditions.

    Read more
    Show Less

    511

    Loading Unit : Loading Method

    Electromagnetic force

    Indenter : Upper pressure indenter

    Type: Flat indenter (50 µm diameter)
    (500 µm flat indenter as option)
    Material: Diamond

    External Dimensions

    Tester: Approx. W 355 × D 405 × H 530 mm Control unit: Approx. W 315 × D 375 × H 110 mm

    Utilities : Humidity

    80% max. (no condensation)

    Utilities : Vibration

    Horizontal vibration: 0.017 Gal max. (at 10 Hz or more)
    0.01 µm max. (at less than 10 Hz)
    Vertical vibration: 0.010 Gal max. (at 10 Hz or more)
    0.005 µm max. (at less than 10 Hz)

    Utilities : Temperature

    Recommended temperature: 23 ± 1°C Allowable range: 10°C to 35°C

    Utilities : Grounding*1

    The grounding pins of 3-pin connectors must be connected to a resistance of 100 W or less.

    Utilities : Power Consumption

    Approx. 100 W (not including power consumption of PC)

    Available test parameters : Test mode

    Single phase AC 100–115 V ± 10%, AC 230 V ± 10% (Ground resistance 100 Ω max.)

    Available test parameters : Test mode

    Calculation of compressive strength, display of test parameters and results
    Display of test force and displacement data
    Display of test force/displacement curve
    Display of test force/displacement identification value
    Display of strength/particle diameter curve
    Display of displacement/time curve
    Display of strength/parameter curve

    Available test parameters : Test mode

    Particle, fiber or other shapes

    Available test parameters : Test mode

    Compression test, load-unload test, cyclic test

    Specimen stage : Horizontal positioning range

    25 mm for both X and Y directions
    Min. increment: 0.01 mm (0.001 mm with option)

    Specimen Stage : Area

    Approx. W 125 mm × D 125 mm

    Specimen stage : Vertical positioning range

    Approx. 60 mm

    Indenter : Lower pressure plate

    SKS flat plate (Diamond pressure plate available as option)

    Optical Head : Min. increment

    0.01 µm / pulse

    Loading unit : Loading range (mN)

    9.8 – 4903

    Optical monitor : Total magnification

    Approx. × 100, × 500 (× 200, × 400, × 1000 with option)

    Loading unit : Load Accuracy

    Within ± 1% of displayed test force or 0.1 mN (whichever is greater)

    Loading unit : Resolution (µm)

    5 (when testing at 49 mN or less)

    Displacement measurement unit : Method

    Differential transformer

    Displacement measurement unit : Method

    0 – 10

    Displacement measurement unit : Method

    0.0001

    Displacement measurement unit : Method

    Within ± 2% of full scale

    Optical Monitor : Objective Lens

    × 10, × 50 (× 20, × 40, × 100 with option)

    Optical Head : Effective measurement range

    Approx. 200 µm (with × 50 objective lens)

    Optical Monitor : Eyepiece

    × 10

    Optical monitor : Illumination method

    Epiluminescent

    Optical monitor : Illumination method

    LED 3 W / 3 V

    Optical monitor : Light path

    Switching between observation and photography possible

    Optical Head : Collimation method

    Direct connection between encorder and control handle: synchronized movement of two indexes

    Optical Head : Detector

    Optical encoder

    Weight

    Tester: Approx. 60 kg Control unit: Approx. 5 kg

    *1 This product is a precision measuring device. Special consideration is required for the product's installation conditions.

    Read more
    Show Less

    210

    Loading Unit : Loading Method

    Electromagnetic force

    Indenter : Upper pressure indenter

    Type: Flat indenter (50 µm diameter)
    (500 µm flat indenter as option)
    Material: Diamond

    External Dimensions

    Tester: Approx. W 355 × D 405 × H 530 mm Control unit: Approx. W 315 × D 375 × H 110 mm

    Utilities : Humidity

    80% max. (no condensation)

    Utilities : Vibration

    Horizontal vibration: 0.017 Gal max. (at 10 Hz or more)
    0.01 µm max. (at less than 10 Hz)
    Vertical vibration: 0.010 Gal max. (at 10 Hz or more)
    0.005 µm max. (at less than 10 Hz)

    Utilities : Temperature

    Recommended temperature: 23 ± 1°C Allowable range: 10°C to 35°C

    Utilities : Grounding*1

    The grounding pins of 3-pin connectors must be connected to a resistance of 100 W or less.

    Utilities : Power Consumption

    Approx. 100 W (not including power consumption of PC)

    Available test parameters : Test mode

    Single phase AC 100–115 V ± 10%, AC 230 V ± 10% (Ground resistance 100 Ω max.)

    Available test parameters : Test mode

    Calculation of compressive strength, display of test parameters and results
    Display of test force and displacement data
    Display of test force/displacement curve
    Display of test force/displacement identification value
    Display of strength/particle diameter curve
    Display of displacement/time curve
    Display of strength/parameter curve

    Available test parameters : Test mode

    Particle, fiber or other shapes

    Available test parameters : Test mode

    Compression test, load-unload test, cyclic test

    Specimen stage : Horizontal positioning range

    25 mm for both X and Y directions
    Min. increment: 0.01 mm (0.001 mm with option)

    Specimen Stage : Area

    Approx. W 125 mm × D 125 mm

    Specimen stage : Vertical positioning range

    Approx. 60 mm

    Indenter : Lower pressure plate

    SKS flat plate (Diamond pressure plate available as option)

    Optical Head : Min. increment

    0.01 µm / pulse

    Loading unit : Loading range (mN)

    9.8 – 1961

    Optical monitor : Total magnification

    Approx. × 100, × 500 (× 200, × 400, × 1000 with option)

    Loading unit : Load Accuracy

    Within ± 1% of displayed test force or 0.1 mN (whichever is greater)

    Loading unit : Resolution (µm)

    2 (when testing at 19 mN or less)

    Displacement measurement unit : Method

    Differential transformer

    Displacement measurement unit : Method

    0 – 100

    Displacement measurement unit : Method

    0.001

    Displacement measurement unit : Method

    Within ± 2% of full scale

    Optical Monitor : Objective Lens

    × 10, × 50 (× 20, × 40, × 100 with option)

    Optical Head : Effective measurement range

    Approx. 200 µm (with × 50 objective lens)

    Optical Monitor : Eyepiece

    × 10

    Optical monitor : Illumination method

    Epiluminescent

    Optical monitor : Illumination method

    LED 3 W / 3 V

    Optical monitor : Light path

    Switching between observation and photography possible

    Optical Head : Collimation method

    Direct connection between encorder and control handle: synchronized movement of two indexes

    Optical Head : Detector

    Optical encoder

    Weight

    Tester: Approx. 60 kg Control unit: Approx. 5 kg

    *1 This product is a precision measuring device. Special consideration is required for the product's installation conditions.

    Read more
    Show Less

    211

    Loading Unit : Loading Method

    Electromagnetic force

    Indenter : Upper pressure indenter

    Type: Flat indenter (50 µm diameter)
    (500 µm flat indenter as option)
    Material: Diamond

    External Dimensions

    Tester: Approx. W 355 × D 405 × H 530 mm Control unit: Approx. W 315 × D 375 × H 110 mm

    Utilities : Humidity

    80% max. (no condensation)

    Utilities : Vibration

    Horizontal vibration: 0.017 Gal max. (at 10 Hz or more)
    0.01 µm max. (at less than 10 Hz)
    Vertical vibration: 0.010 Gal max. (at 10 Hz or more)
    0.005 µm max. (at less than 10 Hz)

    Utilities : Temperature

    Recommended temperature: 23 ± 1°C Allowable range: 10°C to 35°C

    Utilities : Grounding*1

    The grounding pins of 3-pin connectors must be connected to a resistance of 100 W or less.

    Utilities : Power Consumption

    Approx. 100 W (not including power consumption of PC)

    Available test parameters : Test mode

    Single phase AC 100–115 V ± 10%, AC 230 V ± 10% (Ground resistance 100 Ω max.)

    Available test parameters : Test mode

    Calculation of compressive strength, display of test parameters and results
    Display of test force and displacement data
    Display of test force/displacement curve
    Display of test force/displacement identification value
    Display of strength/particle diameter curve
    Display of displacement/time curve
    Display of strength/parameter curve

    Available test parameters : Test mode

    Particle, fiber or other shapes

    Available test parameters : Test mode

    Compression test, load-unload test, cyclic test

    Specimen stage : Horizontal positioning range

    25 mm for both X and Y directions
    Min. increment: 0.01 mm (0.001 mm with option)

    Specimen Stage : Area

    Approx. W 125 mm × D 125 mm

    Specimen stage : Vertical positioning range

    Approx. 60 mm

    Indenter : Lower pressure plate

    SKS flat plate (Diamond pressure plate available as option)

    Optical Head : Min. increment

    0.01 µm / pulse

    Loading unit : Loading range (mN)

    9.8 – 1961

    Optical monitor : Total magnification

    Approx. × 100, × 500 (× 200, × 400, × 1000 with option)

    Loading unit : Load Accuracy

    Within ± 1% of displayed test force or 0.1 mN (whichever is greater)

    Loading unit : Resolution (µm)

    2 (when testing at 19 mN or less)

    Displacement measurement unit : Method

    Differential transformer

    Displacement measurement unit : Method

    0 – 10

    Displacement measurement unit : Method

    0.0001

    Displacement measurement unit : Method

    Within ± 2% of full scale

    Optical Monitor : Objective Lens

    × 10, × 50 (× 20, × 40, × 100 with option)

    Optical Head : Effective measurement range

    Approx. 200 µm (with × 50 objective lens)

    Optical Monitor : Eyepiece

    × 10

    Optical monitor : Illumination method

    Epiluminescent

    Optical monitor : Illumination method

    LED 3 W / 3 V

    Optical monitor : Light path

    Switching between observation and photography possible

    Optical Head : Collimation method

    Direct connection between encorder and control handle: synchronized movement of two indexes

    Optical Head : Detector

    Optical encoder

    Weight

    Tester: Approx. 60 kg Control unit: Approx. 5 kg

    *1 This product is a precision measuring device. Special consideration is required for the product's installation conditions.

    Read more
    Show Less

    MCT Series

    Required PC Specifications

    OS

    Windows 7 (32/64 bit edition)

    CPU

    1 GHz min.

    Disk Drives

    CD-ROM drive

    Display Resolution

    1024 × 768 min.

    Expansion Bus

    PCI Express ×1, 2 slots min.

    Read more
    Show Less

    MCT-510

    Loading Method

    Electromagnetic loading method

    Test force range (mN)

    9.8 to 4903

    Displacement measurement range (µm)

    0 to 100

    MCT-511

    Loading Method

    Electromagnetic loading method

    Test force range (mN)

    9.8 to 4903

    Displacement measurement range (µm)

    0 to 10

    MCT-210

    Loading Method

    Electromagnetic loading method

    Test force range (mN)

    9.8 to 1961

    Displacement measurement range (µm)

    0 to 100

    MCT-211

    Loading Method

    Electromagnetic loading method

    Test force range (mN)

    9.8 to 1961

    Displacement measurement range (µm)

    0 to 10