0

    Measurement of Separator Contraction Behavior (TMA)

    The TMA-60 Thermomechanical Analyzer is an effective tool for evaluation of the expansion and contraction behaviors of separators and other battery materials under heating.

    The contraction behavior was measured for two types of separators (1 and 2) extracted from lithium ion batteries.

    Sample 1 contracts in a higher temperature range than Sample 2.

    batteries-fuel-cells-tma-measure.png

    TMA-60 Thermomechanical Analyzer

    batteries-fuel-cells-tma-60t.png

    An effective tool for evaluation of the expansion and contraction behaviors of separators and other battery materials under heating. The new digital displacement sensor reduces temperature drift to achieve stable measurements. Achieves excellent linearity despite the wide ±5 mm measurement range.